XU Yongchao, SUN Jiabao, ZHAN Hao, FU Binjie, ZHAN Youji, ZHENG Tianqing. Performance of thermal field-assisted precision lapping for single crystal sapphire wafers[J]. Diamond & Abrasives Engineering, 2023, 43(5): 649-656. doi: 10.13394/j.cnki.jgszz.2022.0203
Citation: XU Yongchao, SUN Jiabao, ZHAN Hao, FU Binjie, ZHAN Youji, ZHENG Tianqing. Performance of thermal field-assisted precision lapping for single crystal sapphire wafers[J]. Diamond & Abrasives Engineering, 2023, 43(5): 649-656. doi: 10.13394/j.cnki.jgszz.2022.0203

Performance of thermal field-assisted precision lapping for single crystal sapphire wafers

doi: 10.13394/j.cnki.jgszz.2022.0203
More Information
  • Received Date: 2022-11-19
  • Accepted Date: 2023-02-10
  • Rev Recd Date: 2023-01-29
  • Available Online: 2023-12-07
  • To address the issues of poor surface quality and low efficiency in conventional sapphire wafer lapping processing, a thermal field-assisted processing technology was proposed. The influence of thermal field-assistance on sapphire wafer lapping performance was investigated. While controlling the temperature of the processing area with a self-designed thermal field-assisted device, the lapping tests of sapphire wafers were performed under different processing area temperatures using a semi-fixed flexible machining tool. The effect of processing area temperature on lapping performance was thoroughly examined, along with the material removal mechanism. The simulation results show that the processing area can be quickly heated by a self-designed thermal field-assisted device, and the temperature difference between different areas of the wafer is less than 1.3℃. When the processing area temperature was controlled at 50℃, the surface roughness of sapphire wafers decreased by 6%, and the material removal rate (MRR) improved by nearly 114.2% compared to room temperature. The wear debris test results show that with the increase in processing area temperature during the removal process, the crystal structure of the wafer surface material changed, leading to an improved hydration reaction rate during processing and resulting in a high MRR. Thermal field-assisted precision lapping of sapphire wafers can achieve high surface quality while also increasing processing efficiency, which has a wide range of applications.

     

  • loading
  • [1]
    LI Z, DENG Z, HU Y. Effects of polishing parameters on surface quality in sapphire double-sided CMP [J]. Ceramics International,2020,46(9):13356-13364. doi: 10.1016/j.ceramint.2020.02.116
    [2]
    LYE C S M, WANG Z, LAM Y C. Multi-Foci division of nonlinear energy absorption on ultrashort pulse laser singulation of sapphire wafers [J]. Micromachines,2021,12(11):1328. doi: 10.3390/mi12111328
    [3]
    ZHANG Z, LIU J, HU W, et al. Chemical mechanical polishing for sapphire wafers using a developed slurry [J]. Journal of Manufacturing Processes,2021,62:762-771. doi: 10.1016/j.jmapro.2021.01.004
    [4]
    BHATTACHARYA M, DEY A, MUKHOPADHYAY A K. Influence of loading rate on nanohardness of sapphire [J]. Ceramics International,2016,42(12):13378-13386. doi: 10.1016/j.ceramint.2016.05.091
    [5]
    SHI X, PAN G, ZHOU Y, et al. A study of chemical products formed on sapphire (0001) during chemical-mechanical polishing [J]. Surface and Coatings Technology,2015,270:206-220. doi: 10.1016/j.surfcoat.2015.02.053
    [6]
    万林林, 戴鹏, 刘志坚, 等. 蓝宝石超精密研磨加工研究进展 [J]. 兵器材料科学与工程,2018,41(1):115-123. doi: 10.14024/j.cnki.1004-244x.20180102.004

    WAN Linlin, DAI Peng, LIU Zhijian, et al. Research progress in ultra-precision lapping process of sapphire [J]. Ordnance Material Science and Engineering,2018,41(1):115-123. doi: 10.14024/j.cnki.1004-244x.20180102.004
    [7]
    杨建东, 朱艳秋, 任长根, 等. 机械密封研磨磨具均匀磨损探讨 [J]. 农业机械学报,1998(1):109-113. doi: 10.3969/j.issn.1000-1298.1998.01.023

    YANG Jiandong, ZHU Yanqiu, REN Changgen, et al. Probing lapping tool well-distributed wear in lapping mechanical seals [J]. Transactions of the Chinese Society for Agricultural Machinery,1998(1):109-113. doi: 10.3969/j.issn.1000-1298.1998.01.023
    [8]
    杨建东, 田春林, 金海峰. 固着磨料研磨对工件表面残余应力的影响 [J]. 中国表面工程,2002(4):37-38. doi: 10.3321/j.issn:1007-9289.2002.04.008

    YANG Jiandong, TIAN Chunlin, JIN Haifeng. Effect of solid abrasive lapping on residual surface stress [J]. China Surface Engineering,2002(4):37-38. doi: 10.3321/j.issn:1007-9289.2002.04.008
    [9]
    朱永伟, 付杰, 居志兰, 等. 材料特性对亲水性固结磨料研磨垫加工性能的影响 [J]. 纳米技术与精密工程,2013,11(1):51-56. doi: 10.13494/j.npe.2013.010

    ZHU Yongwei, FU Jie, JU Zhilan, et al. Influence of material characteristics on machining performance of hydrophilic fixed abrasive pad [J]. Nanotechnology and Precision Engineering,2013,11(1):51-56. doi: 10.13494/j.npe.2013.010
    [10]
    林智富, 高尚, 康仁科, 等. 固结金刚石研磨盘加工蓝宝石基片的磨削性能研究 [J]. 人工晶体学报,2016,45(5):1317-1322. doi: 10.3969/j.issn.1000-985X.2016.05.030

    LIN Zhifu, GAO Shang, KANG Renke, et al. Research on grinding performance of fixed-abrasive diamond lapping plates for sapphire substrates [J]. Journal of Synthetic Crystals,2016,45(5):1317-1322. doi: 10.3969/j.issn.1000-985X.2016.05.030
    [11]
    臧江龙. 单晶蓝宝石基片固结磨料机械化学抛光技术 [D]. 大连: 大连理工大学, 2013.

    ZANG Jianglong. Fixed abrasive mechanical chemical polishing of single crystal sapphire substrate [D]. Dalian: Dalian University of Technology, 2013.
    [12]
    LU J, LUO Q, XU X, et al. Removal mechanism of 4H- and 6H-SiC substrates (0001 and 0001) in mechanical planarization machining [J]. Proceedings of the Institution of Mechanical Engineers, Part B: Journal of Engineering Manufacture,2019,233(1):69-76. doi: 10.1177/0954405417718595
    [13]
    GIORDANO F R, FOX W P, HORTON S B. A first course in mathematical modeling [M]. Stamford: Cengage Learning, 2013.
    [14]
    LI J, WANG Z P, LIU W X, et al. Numerical simulation of tire steady-state temperature field based on ANSYS workbench [J]. Key Engineering Materials,2012,501:382-387. doi: 10.4028/www.scientific.net/KEM.501.382
    [15]
    WANG X, LEI H, CHEN R. CMP behavior of alumina/metatitanic acid core-shell abrasives on sapphire substrates [J]. Precision Engineering,2017,50:263-268. doi: 10.1016/j.precisioneng.2017.05.013
    [16]
    XIE W, ZHANG Z, LIAO L, et al. Green chemical mechanical polishing of sapphire wafers using a novel slurry [J]. Nanoscale,2020,12(44):22518-22526. doi: 10.1039/D0NR04705H
    [17]
    赵之琳, 李薇薇, 钱佳, 等. 不同粒径纳米二氧化硅磨料对蓝宝石CMP去除机制的影响 [J]. 电镀与涂饰,2021,40(9):720-725. doi: 10.19289/j.1004-227x.2021.09.013

    ZHAO Zhilin, LI Weiwei, QIAN Jia, et al. Removal mechanism of sapphire during CMP using nano-silica abrasives with different sizes [J]. Electroplating & Finishing,2021,40(9):720-725. doi: 10.19289/j.1004-227x.2021.09.013
    [18]
    XU Y, ZHAO G, WANG Q, et al. Synthesis of Al2O3/SiO2 core-shell composite abrasives toward ultrasmooth and high-efficiency polishing for sapphire wafers [J/OL]. Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering,(2022-11-19) [2022-09-21].https://journals.sagepub.com/doi/10.1177/09544089221124226
    [19]
    冯军. 水合辅助超声磨料流抛光蓝宝石微腔体技术研究 [D]. 长春: 吉林大学, 2019.

    FENG Jun. Hydration-assisted ultrasonic abrasive flow polishing technology on sapphire microcavity [D]. Changchun: Jilin University, 2019.
  • 加载中

Catalog

    通讯作者: 陈斌, bchen63@163.com
    • 1. 

      沈阳化工大学材料科学与工程学院 沈阳 110142

    1. 本站搜索
    2. 百度学术搜索
    3. 万方数据库搜索
    4. CNKI搜索

    Figures(12)  / Tables(2)

    Article Metrics

    Article views (261) PDF downloads(27) Cited by()
    Proportional views
    Related

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return